Peace of mind

12 Step
Finishing Process

  • 1

    Machine and Hand-Sanding
    (both sides)

  • 2

    Machine and Hand-Wiped Stain
    (both sides)

  • 3

    Sealer Coat (front)

  • 4

    Oven Baking #1 (back)

  • 5

    Sealer Coat (back)

  • 6

    Oven Baking #2  (front)

  • 7

    Hand-Sanding (back)

  • 8

    Top Coat (back)

  • 9

    Oven Baking #3 (back)

  • 10

    Hand-Sanding (front)

  • 11

    Top Coat (front)

  • 12

    Oven Baking #4

Super Durable Finishing Process

Huntwood’s exclusive 12-step finishing process is the toughest and longest lasting in the cabinet industry. Hand wiped stain assures consistency and quality. Product goes through 4 coats of sealer and 4 oven chambers to provide maximum cure of the finish.

Catalyzed Conversion Varnish Finish

Our sealer and top coat feature 33% higher solids than the industry standard, providing the ultimate in durability. A catalyst in the sealer is activated in the oven chambers, creating a better cure & harder surface.

Award Winning Process

Our finishing process won the SCAPCA Clean Air Award for its ultra low VOC emissions. Excess materials from paint process are recycled with 80% reused in future applications.

Waste Reutilization

Excess materials are recycled, with 80% reused in future applications.